Oxford Alloy 67 is used for oxyacetylene and gas-tungsten-arc welding of Monel® alloy 450. This alloy is also used for welding on 70/30, 80/20, and 90/10 copper-nickel alloys. The weld metal of this filler metal has excellent resistance to corrosion in sea water, and is widely used for marine and desalination applications. Dissimilar welding applications for Oxford Alloy 67 are joints between Monel® alloys or Nickel 200 and copper-nickel alloys
- 100% argon shielding gas for TIG (GTAW)
- 75% argon/25% helium or 100% argon shielding gas GMAW (MIG)
- 15 - 20 volt GTAW (TIG), 28 - 30 volt (SAW)
Oxford Alloys® 673/32X36 Nickel Bare Rod, Diameter: 3/32 Inch, Length: 36 Inch, Amperage: 120 - 175 amp GTAW (TIG), 275 - 350 amp (SAW), AWS Class: AWS 5.7: ERCuNi, Metallic Luster, Tensile Strength: 53000 psi, Yield Strength: 21000 psi, Elongation in 2" (%): 32%, Welding Process: TIG (GTAW)/MIG/SAW, Weld Metal Composition: 29.0 - 32.0% Nickel (Ni) + Cobalt (Co), 1.0% Manganese (Mn), 0.40 - 0.75% Iron (Fe), 0.25% Silicon (Si), Balanced Copper (Cu) + Silver (Ag), 0.20 - 0.50% Titanium (Ti), 0.02% Phosphorus (P), 0.02% Lead (Pb), 0.50% OET, Applicable Materials: 70/30, 80/20, 90/10 Copper-Nickel Alloys, Monel® Alloy 450, Nickel 200 And Copper-Nickel Alloys