Welcome to Gas and Supply.
Need help? Call toll free 1 (844) 840-4427

Quick Order| Locations| SDS| About Us| Careers| Contact Us
< Back to catalog
Oxford Alloys 60 Metallic Luster Ernicu-7 Nickel Bare Rod, 1/8 Inch Dia. X 36 Inch L 601/8X36 OXF601/8X36

Detailed Description

Oxford Alloy 60 is used for the welding of Monel® alloys 400, R-405, and K-500. This filler metal is also used for surfacing of steel. The weld metal deposited by the Oxford Alloy 60 has properties similar to those of Monel® alloy 400. This filler metal has good strength and resists corrosion in many media, including seawater, salts, and reducing acids. The weld metal of the Oxford Alloy 60 is not age hardenable and when used to join Monel® alloy K-500 it has lower strength than the base metal

Features
  • 100% argon shielding gas for TIG (GTAW)
  • 75% argon/25% helium or 100% argon shielding gas GMAW (MIG)
  • 15 - 20 volt GTAW (TIG), 29 - 32 volt (SAW)

Oxford Alloys® 601/8X36 Nickel Bare Rod, Diameter: 1/8 Inch, Length: 36 Inch, Amperage: 150 - 220 amp GTAW (TIG), 350 - 450 amp (SAW), AWS Class: AWS 5.14: ERNiCu-7, Metallic Luster, Tensile Strength: 76500 psi, Yield Strength: 52500 psi, Elongation in 2" (%): 34%, Welding Process: TIG (GTAW)/MIG/SAW, Weld Metal Composition: 62.0 - 69.0% Nickel (Ni), 0.15% Carbon (C), 4.0% Manganese (Mn), 2.5% Iron (Fe), 1.25% Silicon (Si), Balanced Copper (Cu), 1.25% Aluminum (Al), 1.5 - 3.0% Titanium (Ti), 0.02% Phosphorus (P), 0.015% Sulphur (S), 0.50% OET, Applicable Materials: Monel® Alloys 400, R-405, And K-500 Nickel Alloy, Steel

Technical Details

Amperage
150 - 220 amp GTAW (TIG), 350 - 450 amp (SAW)
Applicable Materials
Monel® Alloys 400, R-405, And K-500 Nickel Alloy, Steel
AWS Class
AWS 5.14: ERNiCu-7
Color
Metallic Luster
Diameter
1/8 Inch
Elongation in 2" (%)
34%
Length
36 Inch
Tensile Strength
76500 psi
Weld Metal Composition
62.0 - 69.0% Nickel (Ni), 0.15% Carbon (C), 4.0% Manganese (Mn), 2.5% Iron (Fe), 1.25% Silicon (Si), Balanced Copper (Cu), 1.25% Aluminum (Al), 1.5 - 3.0% Titanium (Ti), 0.02% Phosphorus (P), 0.015% Sulphur (S), 0.50% OET
Welding Process
TIG (GTAW)/MIG/SAW
Yield Strength
52500 psi