Bohler Thyssen Bohler 112 Ernicrmo-3 3/16 Dia 12.3 # Per Can 36.9# Per Cs 80117 BOH80117

Detailed Description

Nickel base electrode, high resistance to corrosive environments. Resistant to stress corrosion cracking. Resistant to scaling up to 2,012°F. Temperature limit: 932°F max. in sulphureous atmospheres. Creep resistant up to 1,832°F. Cold toughness down to -321°F. For joining and surfacing with matching/similar corrosion resistant materials as well as on matching and similar heat resistant, creep resistant steels and alloys, cryogenic austenitic CrNi(N) steels/cast steel grades and cryogenic Ni steels suitable for quenching and tempering.

Technical Details

Heat treatment: as welded YS 61 ksi UTS 110 ksi Elong 30% CVN 55 ft-lb @ 68°F 44 ft-lb @ -320°F