Techalloy® 55 is used for welding of cast irons to other cast irons as well as for joining cast irons to mild steels. It is also readily used for the repair of castings. The welds are moderately hard and require carbide tipped tools for machining. A preheat and inter-pass temperature of not less than 350 deg F (175 deg C) is required during welding to prevent cracking
Techalloy® MG55045667 Nickel Alloy Welding Wire, Solid, Gas Shielded, Diameter: 3/64 Inch, Amperage: 150 - 190 amp, Package: 33 lb Wire Basket, AWS Class: AWS A5.15: ENiFe-CI, Welding Process: MIG (GMAW And SAW), Weld Metal Composition: 0.01% Carbon (C), 0.5% Manganese (Mn), 0.1% Silicon (Si), 0.002% Sulphur (S), 44.5% Iron (Fe), 54% Nickel (Ni), 0.02% Copper (Cu), 0.005% Aluminum (Al)