Oxford Alloys Copper Coated Solid Er70s-6 Mild And Low Alloy Steel Welding Wire, 0.035 Inch Dia., 33 Lb Spool 70S-6.035X33 OXF70S-6.035X33

Detailed Description

Features

  • Oxford alloy ER70S-6 contains high levels of manganese and silicon for stronger de-oxidizing power where stringent cleaning procedures are not possible
  • The high silicon content increases the fluidity of the weld pool, creating a smoother bead appearance and resulting in minimal post-weld grinding
  • The Oxford Alloy ER70S-6 has been designed to provide X-ray quality porosity-free welds and the highest tensile strength (as welded) of the plain carbon steel wires
  • 100 - 290 in./min. wire feed speed
  • 20 ft-lb at -20 deg F impact strength

 

Oxford Alloys 70S-6.035X33 Mild And Low Alloy Steel Welding Wire, Solid, Diameter: 0.035 Inch, Current Type: DC+, Package: 33 lb Spool, AWS Class: AWS A5.18: AWS ER70S-6, Copper-Coated, Tensile Strength: 79750 psi, Yield Strength: 65250 psi, Elongation in 2" (%): 30%, Welding Process: MIG (GMAW And SAW)/TIG/SUB-ARC Wire, Weld Metal Composition: 0.06-0.15% Carbon (C), 1.4-1.85% Manganese (Mn), 0.8-1.15% Silicon (Si), 0.025% Phosphorus (P), 0.035% Sulphur (S), 0.15% Nickel (Ni), 0.15% Chromium (Cr), 0.15% Molybdenum (Mo), 0.03% Vanadium (V), 0.5% Copper (Cu)

Technical Details

AWS Class
AWS A5.18: AWS ER70S-6
Current Type
DC+
Diameter
0.035 Inch
Elongation in 2" (%)
30%
Finish/Color
Copper-Coated
Package
33 lb Spool
Tensile Strength
79750 psi
Type
Solid
Weld Metal Composition
0.06-0.15% Carbon (C), 1.4-1.85% Manganese (Mn), 0.8-1.15% Silicon (Si), 0.025% Phosphorus (P), 0.035% Sulphur (S), 0.15% Nickel (Ni), 0.15% Chromium (Cr), 0.15% Molybdenum (Mo), 0.03% Vanadium (V), 0.5% Copper (Cu)
Welding Process
MIG (GMAW And SAW)/TIG/SUB-ARC Wire
Yield Strength
65250 psi