Welcome to Gas and Supply.
Need help? Call toll free 1 (844) 840-4427

Quick Order| Locations| SDS| About Us| Careers| Contact Us
< Back to catalog
Lincoln Superglaze Ed028635 Er70s-6 Mild Steel Welding Wire, 0.035 Inch Dia., 44 Lb Fiber Spool ED028635 LINED028635

Detailed Description

Features
  • Deoxidizers tolerate light mill scale
  • Microguard® ultra provides superior feeding and arc stability
  • Bare wire reduces copper fumes
  • Supports short-circuiting, globular, axial spray and pulsed spray transfer
  • High levels of manganese and silicon deoxidizers tolerate medium to heavy mill scale surfaces
  • Consistent weld deposit chemistry and procedures from package to package improve quality and save time
  • Fluid puddle, good wash-in at weld toes and flat weld beads minimize defects, scrap or re-work
  • Low feed forces reduce wear and tear on gun liners and contact tips
  • All welding positions, 100% Co2, 75 - 95% argon/balance Co2, 95 - 98% argon/balance O2, 30 - 50 cfh flow rate

Lincoln® SuperGlaze® ED028635 Mild Steel Welding Wire, Diameter: 0.035 Inch, Spool Diameter: 12 Inch, Package: 44 lb Fiber Spool, AWS Class: AWS A5.18/A5.18M: 2005: ER70S-6, Tensile Strength: 78 ksi (As Welded), Yield Strength: 62000 psi (As Welded), Elongation in 2" (%): 28% (As Welded), Charpy V-Notch: 27 ft.-lb. At -20 deg F, Welding Process: MIG (GMAW And SAW), Weld Metal Composition: 0.08-0.09% Carbon (C), 1.42-1.65% Manganese (Mn), 0.81-0.87% Silicon (Si), 0.006-0.01% Sulphur (S), 0.004-0.01% Phosphorus (P), 0.01-0.05% Chromium (Cr), ? 0.04% Nickel (Ni), ? 0.01% Molybdenum (Mo), < 0.01% Vanadium (V), 0.01-0.04% Copper (Cu)

Technical Details

AWS Class
AWS A5.18/A5.18M: 2005: ER70S-6
Charpy V-Notch
27 ft.-lb. At -20 deg F
Diameter
0.035 Inch
Elongation in 2" (%)
28% (As Welded)
Package
44 lb Fiber Spool
Spool Diameter
12 Inch
Tensile Strength
78 ksi (As Welded)
Weld Metal Composition
0.08-0.09% Carbon (C), 1.42-1.65% Manganese (Mn), 0.81-0.87% Silicon (Si), 0.006-0.01% Sulphur (S), 0.004-0.01% Phosphorus (P), 0.01-0.05% Chromium (Cr), ? 0.04% Nickel (Ni), ? 0.01% Molybdenum (Mo), < 0.01% Vanadium (V), 0.01-0.04% Copper (Cu)
Welding Process
MIG (GMAW And SAW)
Yield Strength
62000 psi (As Welded)